Sunday, October 2, 2022

Solar Water Tank Leaking problem

We made some analysis based on installation and maintenance experiences as following:

1. Inner tank corrosion

The inner tank corrosion usually caused by local bad water quality, especially in the coastal areas. Cl and SO ion in the water (PPM>180mg/L) would corrode the inner tank.

Solution: replace the tank by S

solar water heater maintenance

US 316L inner material, or use the copper coil close loop thermosiphon system.

Attention area: coastal areas like Netherlands, Belgium, Italy or Mid-east like Jordan, Lebanon, etc.


2. Some of the welding position of the tank break

Some of the welding position of the tank break, especially the inlet/outlet. These breaks can’t be repaired or too expensive to be repaired.

Solution: replace by new tank.


3. Shrunken of the inner tank

Shrunken of the inner tank and which result the twist of the sealing rubber ring or other related outlet parts, the sealing system was damaged to leak. If the heat time is short to the solar water heater, however the water in the tank runs out with not long time, which could be caused by shrunken of the inner tank. The installation personnel without professional training would make the errors that the gas vent blocked or thinned. Elbow or bibcock added to the end of the overflow indoor by the users for beauty without the knowledge that the overflow pipe also has ventilatory function.

Shrunken of the inner tank usually appears in winter. The water level is high, however, the temperature of the original water in the tank is too low, the air vent would be blocked by the ice. Once the inner tank shrunken, the tank scrap.

Solution: ask the distributer to replace a new tank if caused by installation.


4. Sealing rubber ring worn, aged

Sealing rubber ring worn, aged. Clutters stick to the inner circle of the sealing ring would effect the sealing between the sealing rubber ring and the vacuum tube and venting or inlet/outlet components which would cause water seepage.

Solution: replace the sealing rubber ring.

Hot water tank users should treat the leaking phenomenon cautiously. The water would infiltrate into the insulation layer which would make the tank fail to preserve heat.


For more info contact solar water heater maintenance or call us at +971 4 252 2966


Forms of Corrosion Occurs in Stainless Steel


Pitting corrosion - The passive layer on stainless steel can be attacked by certain chemical species. The chloride ion Cl- is the most common of these and is found in everyday materials such as salt and bleach. Pitting corrosion is avoided by making sure that stainless steel does not come into prolonged contact with harmful chemicals or by choosing a grade of steel which is more resistant to attack. The pitting corrosion resistance can be assessed using the Pitting Resistance Equivalent Number calculated from the alloy content.

solar water heater maintenance

Crevice corrosion - Stainless steel requires a supply of oxygen to make sure that the passive layer can form on the surface. In very tight crevices, it is not always possible for the oxygen to gain access to the stainless steel surface thereby causing it to be vulnerable to attack. Crevice corrosion is avoided by sealing crevices with a flexible sealant or by using a more corrosion resistant grade.

General corrosion - Normally, stainless steel does not corrode uniformly as do ordinary carbon and alloy steels. However, with some chemicals, notably acids, the passive layer may be attacked uniformly depending on concentration and temperature and the metal loss is distributed over the entire surface of the steel. Hydrochloric acid and sulphuric acid at some concentrations are particular aggressive towards stainless steel.


Stress corrosion cracking (SCC) - This is a relatively rare form of corrosion which requires a very specific combination of tensile stress, temperature and corrosive species, often the chloride ion, for it to occur. Typical applications where SCC can occur are hot water tanks and swimming pools. Another form known as sulphide stress corrosion cracking (SSCC) is associated with hydrogen sulphide in oil and gas exploration and production.


Intergranular corrosion - This is now quite a rare form of corrosion. If the Carbon level in the steel is too high, Chromium can combine with Carbon to form Chromium Carbide. This occurs at temperatures between about 450-850 deg C. This process is also called sensitisation and typically occurs during welding. The Chromium available to form the passive layer is effectively reduced and corrosion can occur. It is avoided by choosing a low carbon grade the so-called 'L' grades or by using a steel with Titanium or Niobium which preferentially combines with Carbon.


Galvanic corrosion - If two dissimilar metals are in contact with each other and with an electrolyte e.g. water or other solution, it is possible for a galvanic cell to be set up. This is rather like a battery and can accelerate corrosion of the less 'noble' metal. It can avoided by separating the metals with a non-metallic insulator such as rubber.


For more info contact solar water heater maintenance or call us at +971 4 252 2966

Freeze Protection Measures in Solar Water Heating Systems

In regions with cold winters, protecting solar water heating systems from freezing is crucial to ensure continuous operation and prevent dam...